A TEM investigation on precipitation behavior of AEREX350 superalloy
Sarmee, M ; Sharif University of Technology | 2008
298
Viewed
- Type of Document: Article
- DOI: 10.7449/2008/Superalloys_2008_549_552
- Publisher: 2008
- Abstract:
- The influence of solution treatment on precipitation behavior of AEREX™350 was investigated using hardness testing, TEM and SEM. Samples were solution treated at 1050°C and 1075°C for 1 hr and then aged at 700°C, 750°C and 800°C for 1,2,4,8 and 25 hrs. It was found that different solution treatment may be used for different applications of AEREX™350
- Keywords:
- Hardness testing ; Precipitation behavior ; Sem ; Solution treatment ; Tem ; Superalloys ; AEREX350 superalloy ; Precipitation
- Source: 11th International Symposium on Superalloys, Superalloys 2008, Champion, PA, 14 September 2008 through 18 September 2008 ; January , 2008 , Pages 549-552
- URL: https://www.tms.org/Superalloys/10.7449/2008/Superalloys_2008_549_552.pdf