A TEM investigation on precipitation behavior of AEREX350 superalloy
, Article 11th International Symposium on Superalloys, Superalloys 2008, Champion, PA, 14 September 2008 through 18 September 2008 ; January , 2008 , Pages 549-552 ; Asgari, S ; Sharif University of Technology
2008
Abstract
The influence of solution treatment on precipitation behavior of AEREX™350 was investigated using hardness testing, TEM and SEM. Samples were solution treated at 1050°C and 1075°C for 1 hr and then aged at 700°C, 750°C and 800°C for 1,2,4,8 and 25 hrs. It was found that different solution treatment may be used for different applications of AEREX™350