This study has investigated the effects of different environmental conditions on the bond at the interface between two fiber reinforced polymer (FRP) layers. A total of 945 single lap splice coupons with three bond length were made using wet lay-up technic. There were used three unidirectional fabrics and one type of epoxy resin. A Uniaxial tensile test was performed on samples after 2, 4, 12, 20, 28, 36 and 48 weeks of exposure. Also series of test were conducted in order to determine the minimum lap splice length of single splice FRP samples. The experimental results indicated reduction of bond strength in glass specimens that was 17 % after 48 weeks of exposure while for same amount of...
This study has investigated the effects of different environmental conditions on the bond at the interface between two fiber reinforced polymer (FRP) layers. A total of 945 single lap splice coupons with three bond length were made using wet lay-up technic. There were used three unidirectional fabrics and one type of epoxy resin. A Uniaxial tensile test was performed on samples after 2, 4, 12, 20, 28, 36 and 48 weeks of exposure. Also series of test were conducted in order to determine the minimum lap splice length of single splice FRP samples. The experimental results indicated reduction of bond strength in glass specimens that was 17 % after 48 weeks of exposure while for same amount of...