Removal of Non-Metallic Inclusions from Nickel Base Superalloys by Electromagnetic Levitation Melting in a Slag
, M.Sc. Thesis Sharif University of Technology ; Halali, Mohammad (Supervisor)
Abstract
Samples of INCONEL 718 were levitated and melted in a slag by the application of an electromagnetic field. The effects of temperature, time and slag composition on the inclusion content of the samples were studied thoroughly. Samples were compared with the original alloy to study the effect of the process on inclusions. Size, shape and chemical composition of remaining nonmetallic inclusions were investigated. The samples were prepared by Standard Guide for Preparing and Evaluating Specimens for Automatic Inclusion Assessment of Steel (ASTM E 768-99) method and the results were reported by means of the Standard Test Methods for Determining the Inclusion Content of Steel (ASTM E 45-97)....
Role of base-metal composition in isothermal solidification during diffusion brazing of nickel-based superalloys
, Article Science and Technology of Welding and Joining ; Volume 23, Issue 1 , 2018 , Pages 13-18 ; 13621718 (ISSN) ; Ekrami, A ; Kokabi, A. H ; Sharif University of Technology
Taylor and Francis Ltd
2018
Abstract
The key feature of diffusion brazing, also referred to as transient liquid phase bonding, is isothermal solidification which precludes the formation of intermetallic in the joint centreline. Analysing the available data published in the literature showed that the composition of the nickel-based superalloys plays a strong role in determining the required time for obtaining intermetallic-free joint during diffusion brazing. This effect is not predictable by the standard conventional models. It is proposed that increasing the boride-forming elements in the base superalloy which promotes in situ boride precipitation at the diffusion-affected zone can accelerate the diffusion flux of the boron...
Intermetallic phase formation during brazing of a nickel alloy using a Ni–Cr–Si–Fe–B quinary filler alloy
, Article Science and Technology of Welding and Joining ; Volume 24, Issue 4 , 2019 , Pages 342-351 ; 13621718 (ISSN) ; Pouranvari, M ; Sharif University of Technology
Taylor and Francis Ltd
2019
Abstract
Fundamental understanding of the intermetallic phase formation is the key for enhancing the robustness and reliability of the brazed joints. The paper addresses the phase transformations during brazing of the Hastelloy X nickel-base superalloy using the quinary Ni–13Cr–4.5Si–4.2Fe–2.8B (wt-%) braze alloy. The mechanisms of intermetallic formation via solidification and solid-state precipitation are discussed. The athermal solidification zone (ASZ) is featured by the formation of brittle and hard borides and boro-silicides that are formed via eutectic reactions. However, in contrast to other commercial B-bearing Ni-based filler alloys, it was identified that the presence of a high-volume...
Remelting of Nickael Based Superalloy (IN738LC) and its Effect on the Physical Metallurgy and Microstructure
, M.Sc. Thesis Sharif University of Technology ; Yoozbashizadeh, Hossein (Supervisor)
Abstract
Well worn gas turbine blade made of Nickel based superalloy, IN738LC was remelted due to remove inclusion and use it in casting process of new blade after microstrucrure investigation in neutral atmosphere and vacuum. The composition of slags for removing inclusions used for this practice were 70CaF2-20CaO-10Al2O3 and 55CaO-45Al2O3. The microstructural characterization involved use both optical as well as electron microscope including application of EDS technique for denoted the type of carbides and inclusion investigation. Chemical composition was determined by despersive spectroscopy method. The changing in main elements were reported too low. Number of inclusions were decreased in the...
Experimental Study of Pendulum Grinding of Superalloys
, M.Sc. Thesis Sharif University of Technology ; Akbari, Javad (Supervisor)
Abstract
Superalloys are widely used in aerospace and power industries due to the good performance at high temperatures for examples gas turbines, steam turbines and aircraft components. In addition to the turbines cobalt-base superalloys are used in medical implants such as knee and hip joints. The main strengths of the superalloys are heat-resistant, retaining their high mechanical and chemical properties at high temperatures, high melting temperatures, high corrosion resistance, resistance to thermal fatigue, thermal shock, creep, and erosion. Because of difficult to machine properties of superalloys, grinding is one of the effective methods for machining superalloys. The surface integrity of the...
The Making of Vacuum Induction Melting Furnace and the Survey of the Influences of Temperature and Material of Crucible on Created Type of Inclusion in Super Alloyed Based Nickel IN738LC
, M.Sc. Thesis Sharif University of Technology ; Halali, Mohammad (Supervisor)
Abstract
The purpose of this project is to survey the created kind of inclusion in super alloyed based nickel. primarily, for this matter for the preparing of super alloyed based nickel, the vacuum induction melting furnace has been designed and built , then for surveying the kind of inclusion the effective parameters such as temperature , timing and material of crucible has been considered accordingly , the material of crucibles was considered based on mud-clay- graphitic- pure graphitic- aluminum- zirconium. From the obtained analysis samples of SEM has been distinguished which, with increasing of the temperature and the time ,the percentage of impurity will go up in super- alloyed and the...
Mechanical Properties of Two-Phase Microstructure in Nickel Based Superalloys with Molecular Dynamics Method
, M.Sc. Thesis Sharif University of Technology ; Khoei, Amir Reza (Supervisor)
Abstract
Nickel based superalloys are widely used in turbines since they are highly resistant to static, fatigue and creep loadings at high temperatures. Efficiency of turbines can be increase by application and development of these materials, which leads to reduced energy consumption. Nickel based superalloys constitutes of two phases, γ and γ' with multiscale behaviour. Thus to better understand the behaviour of this material, its behaviour should be studied across different scales.Molecular dynamics is used to model mechanical behaviour of this superalloy. This method is used for atomistic simulation of materials in which forces between atoms are modelled using an interatomic potential. Different...
Studying of Micro-structure and Mechanical Properties of Resistant Spot Welds of Nickel Base Super Alloys
, M.Sc. Thesis Sharif University of Technology ; Pouranvari, Majid (Supervisor)
Abstract
Resistance spot welding is one of the fabrication processes of gas turbines. Due to few published works about using RSW for joining participation hardened nickel base super alloys like Nimonic C263 and solid solution hardened ones like Hastelloy X, this work tries to investigate the microstructure and mechanical properties of RSW joints of these super alloys. In phase one, effect of welding current on structural properties of welds, hardness profile from the center of the weld to the edge of it, failure mod and failure energy were investigated. In phase two, effect of standard heat treatment of Nimonic C263 and the initial microstructure of the base metal on the micro-structure and...
Study of Microstructural Evolution of AEREX 350 Alloy During High Temperature Ttensile Testing
, M.Sc. Thesis Sharif University of Technology ; Asgari, Sirous (Supervisor)
Abstract
In this study, samples of wrought nickel-cobalt superalloy AEREX350 underwent hot tensile testing at temperatures ranging from 500 to in the solution-treated state, with subsequent investigation into their mechanical properties and microstructural changes. Anomalous yield strength behavior was observed in this alloy, characterized by an initial decrease in yield stress with rising temperature, followed by an increase and subsequent decrease. Similarly, the ultimate tensile strength exhibited a similar trend to the yield stress. Conversely, ductility parameters demonstrated an inverse relationship with alloy strength. Notably, the alloy displayed a pronounced work-hardening rate at 800 °C....
Diffusion induced isothermal solidification during transient liquid phase bonding of cast IN718 superalloy
, Article Canadian Metallurgical Quarterly ; Vol. 53, issue. 1 , 2014 , p. 38-46 ; Ekrami, A ; Kokabi, A. H ; Sharif University of Technology
Abstract
In transient liquid phase (TLP) bonding for commercial applications, one of the important key parameters is the holding time required for complete isothermal solidification tIS, which is a prerequisite for obtaining a proper bond microstructure. The objective of the study is to analyse the isothermal solidification kinetics during TLP bonding of cast IN718 nickel based superalloy. Experiments for TLP bonding were carried out using a Ni-7Cr-4.5Si-3Fe-3.2B (wt-%) amorphous interlayer at several bonding temperatures (1273-1373 K). The time required to obtain TLP joints free from centreline eutectic microconstituents was experimentally determined. Considering the solidification behaviour of...
Phase transformations during diffusion brazing of IN718/Ni-Cr-B/IN718
, Article Materials Science and Technology (United Kingdom) ; Volume 29, Issue 8 , 2013 , Pages 980-984 ; 02670836 (ISSN) ; Ekrami, A ; Kokabi, A. H ; Sharif University of Technology
2013
Abstract
The production of robust joints after diffusion brazing necessitates the advanced understanding of phase transformations during the bonding process. This paper aims to investigate the solidification and the solid state precipitation during diffusion brazing of wrought IN718 nickel base superalloy using Ni-15Cr-4B (wt-%) filler alloy. It was found that intermetallics containing eutectic type microconstituents were formed in the joint centreline by solidification which is controlled by segregation behaviour of B and its low solubility in Ni rich solid solution. In addition, extensive Cr-Mo-Nb rich precipitates were formed in the substrate region by solid state precipitation induced by B...
TLP bonding of cast IN718 nickel based superalloy: Process-microstructure-strength characteristics
, Article Materials Science and Engineering A ; Volume 568 , 2013 , Pages 76-82 ; 09215093 (ISSN) ; Ekrami, A ; Kokabi, A. H ; Sharif University of Technology
2013
Abstract
This paper aims at addressing the microstructure-strength characteristics relationship during transient liquid phase (TLP) bonding of cast IN718 nickel based superalloy using Ni-7. Cr-4.5. Si-3. Fe-3.2. B (wt%) amorphous interlayer. The progress of the isothermal solidification at different temperatures for different times is analyzed using a Larson-Miller parameter (LMP). It was found that there is direct relationship between isothermal solidification zone (ISZ) size and LMP. Results showed that in situation where isothermal solidification has not been completed, the ratio of athermal solidification zone (ASZ) size to the width of the total solidified zone is the controlling factor for...
Laser-assisted friction stir processing of IN738LC nickel-based superalloy:stir processing of IN738LC nickel-based superalloy: Stir zone characteristics.tir zone characteristics
, Article Science and Technology of Welding and Joining ; Volume 21, Issue 5 , 2016 , Pages 374-380 ; 13621718 (ISSN) ; Pouranvari, M ; Ghaini, F. M ; Fujii, H ; Chung, Y. D ; Sharif University of Technology
Taylor and Francis Ltd
Abstract
Friction stir processing (FSP) of high softening-temperature materials such as nickel-based superalloys is considered to be difficult. Laser heating of a localised area ahead of the FSP tool was used to provide sufficient plasticity during the FSP of IN738LC nickel-based superalloy. The stir zone (SZ) microstructure of the friction stir processed and laser-assisted friction stir processed were characterised. Laser-assisted friction stir processing (LAFSP) produced a defect-free pass, but FSP resulted in generation of a discontinuity in the SZ. Both lower volume fraction of partially dissolved γ′ precipitates and coarser grain structure of SZ in LAFSP led to more ductility of the SZ material...
Densification and microstructural evolution during co-sintering of Ni-base superalloy powders
, Article Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science ; Volume 37, Issue 8 , 2006 , Pages 2549-2557 ; 10735623 (ISSN) ; Sharif University of Technology
2006
Abstract
This work presents the effect of co-sintering on the densification and microstructural evolution in the two-layer stepwise graded composite of INCONEL 718 and INCONEL 625 superalloys. A pressureless co-sintering method in conjunction with a powder layering technique was used. The sintering was carried out in solid state and liquid phase in temperature ranging from 1260 °C through 1300 °C for 60 minutes in a low pressure of an argon atmosphere. Nonisothermal sintering behavior was also examined by dilatometric analysis. Similarly, the sintering response of the individual layers was characterized. The results reveal an enhanced densification rate during co-sintering of the composite layers....
On the heat treatment of Rene-80 nickel-base superalloy
, Article Journal of Materials Processing Technology ; Volume 176, Issue 1-3 , 2006 , Pages 240-250 ; 09240136 (ISSN) ; Nategh, S ; Sharif University of Technology
2006
Abstract
Rene-80, as an alloy for production of the jet turbine blades, shows high mechanical properties as well as microstructure stability during the high temperature engine operation. In this study we tried to have a deep insight on the microstructure of the cast Rene-80 and the evolution of microstructure during the different stages of the relatively complex GE class-A heat treatment. Although the solution heat treatment homogenized the chemical alloy segregation resulted from the casting to some extent, it did not cause all the casting γ′ particles to dissolve completely in the matrix. Primary aging caused growth in the residue particles as well as growth of the new precipitated particles, which...
Microstructural evolution mechanism during brazing of Hastelloy X superalloy using Ni–Si–B filler metal
, Article Science and Technology of Welding and Joining ; Volume 23, Issue 5 , 2018 , Pages 441-448 ; 13621718 (ISSN) ; Pouranvari, M ; Sharif University of Technology
Taylor and Francis Ltd
2018
Abstract
The paper aims at understanding solidification phenomena and solid state precipitations during diffusion brazing of Hastelloy X nickel base superalloy using a ternary Ni–4.5Si–3.2 B (in wt-%) filler metal. The joint is featured by the formation of Ni-rich solid solution in an isothermal solidification zone, borides/silicide formation during eutectic-type solidification in an athermal solidification zone, on-cooling precipitation of fine nickel silicides in the joint centerline, in situ precipitation of Mo–Cr-rich borides in the diffusion affected zone and grain growth in the heat affected zone. The implication of the phase transformations on the joint properties is discussed. It is shown...
Thermal processing strategies enabling boride dissolution and gamma prime precipitation in dissimilar nickel-based superalloys transient liquid phase bond
, Article Materials and Design ; Volume 182 , 2019 ; 02641275 (ISSN) ; Pouranvari, M ; Sharif University of Technology
Elsevier Ltd
2019
Abstract
The microstructure of dissimilar transient liquid phase bond between Hastelloy X and IN792 nickel-based superalloys is featured by lack of sufficient formation of γ′ precipitates in the bond-centerline and extensive in-situ precipitation of boride second phases in the diffusion affected zones (DAZ). This paper investigates the impact of two thermal processing strategies, using standard solution treatment and aging of IN792 (STA strategy) and using solution treatment of IN792 followed by a post-bond heat treatment utilizing solution treatment of Hastelloy X and aging treatment of IN792 (SPTA strategy) on the joint microstructure and mechanical properties. The boride precipitates in the DAZ of...
Microstructure Evolution Mechanism and Mechanical Properties of TLP bonded IN718 Nickel Based Superalloy
, Ph.D. Dissertation Sharif University of Technology ; Ekrami, Ali Akbar (Supervisor) ; Kokabi, Amir Hossein (Supervisor)
Abstract
The thesis is focused on the process-microstructure-properties relationships in transient liquid phase (TLP) bonded IN718 nickel based superalloy. The bonding was carried out using Ni-B-(Si)-(Cr) interlayers at temperatures of 1273-1448 K with various bonding time to ensure completion of isothermal solidification. Microstructure development mechanism, kinetics of isothermal solidification during bonding process, influence of microstructure gradient induced by bonding process on the aging behavior of the joint and the response of joint region to post-bonded heat treatment were considered. It was shown that the isothermal solidification rate depends on the (1) diffusion flux of B into the...
Microstructural Study Of Inconel 718 Alloy Produced by VAR and Comparing it with Other Rapid Solidification Methods
, M.Sc. Thesis Sharif University of Technology ; Ashuri, Hossein (Supervisor)
Abstract
The purpose of this investigation was to study the microstructure of the Inconel718 alloy wich was produced by VAR and suction casting method, and study the effect of cooling rate on the solidification structure of Inconel718 alloy. In the first a labratoary scale VAR furnace was made. After producing some sample's with this furnace, a suction casting sample was produced using a 3mm diameter copper mold. Metallography, SEM, EDS, and microhardness analysis was carried away. Cooling rate evaluation was done by using a equation between secondary dendrite arm spacing and solidification time. Results showed that by increasing cooling rate from 63 c/s to around 2000 c/s, columnar and equiaxed...
Investigation of Microstructural Evolutions During Dissimilar TLP Bonding of IN792 and Hastelloy X Nickel Based Superalloys
, M.Sc. Thesis Sharif University of Technology ; Pouranvari, Majid (Supervisor)
Abstract
In this thesis, macrostructural evolutions in dissimilar TLP bonding of as-cast nickel based supperalloy IN792 to wrought HX was investigated. In the first step of this study solidification behavior of Ni-Cr-Fe-Si-B (MBF-15) interlayer in presence of HX as base metal at 1120 °C was surveyed. In second step, bonding of HX/HX, IN792/IN792 and HX/IN792 systems with MBF-15 interlayer at 1120 °C and different times were studied and isothermal solidification time and factors that affect this stage were discussed. In third step, synchronization of dissimilar bonding with standard heat treatment cycle of IN792 was investigated and effect of this cycle on aging response of different zones, isothermal...